(a) SEM image and EDS analysis results of bare alloy 214-7 after 1000 h of exposure to SCW at 700 °C/25 MPa with (b) surface crack magnified for clarity

(a) SEM image and EDS analysis results of bare alloy 214-7 after 1000 h of exposure to SCW at 700 °C/25 MPa with (b) surface crack magnified for clarity