Fretting wear studies were conducted on AZ91 and AE42 magnesium alloys against steel ball. Average coefficient of friction (COF) remains steady with the increase in running time. However, average coefficient of friction decreases with the increase in normal load and frequency and marginally increases with the increase in amplitude. A constant average coefficient of friction of 0.06 was observed for both AZ91 and AE42 under dry sliding conditions at normal load of 50 N. Wear volume increases linearly with increasing running time. Wear volume first decreases sharply, attains minima, and then increases marginally with the increase in normal load. However, wear volume increases with increasing amplitude and frequency. Higher specific wear rate of 10.5 × 10−6 mm3 N−1·m−1 was observed for AE42, as compared to 4.5 × 10−6 mm3 N−1·m−1 for AZ91. The wear in magnesium alloy was caused by a combination of adhesion, abrasion, oxidation, delamination, and plastic deformation under different fretting conditions.
Skip Nav Destination
Article navigation
January 2018
Research-Article
Tribological Characterization of AZ91 and AE42 Magnesium Alloys in Fretting Contact
D. Khabale,
D. Khabale
Tribology Laboratory,
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
Search for other works by this author on:
M. F. Wani
M. F. Wani
Tribology Laboratory,
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
e-mail: mfwani@nitsri.net
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
e-mail: mfwani@nitsri.net
Search for other works by this author on:
D. Khabale
Tribology Laboratory,
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
M. F. Wani
Tribology Laboratory,
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
e-mail: mfwani@nitsri.net
Mechanical Engineering Department,
National Institute of Technology Srinagar,
Hazratbal,
Srinagar 190006, Jammu and Kashmir, India
e-mail: mfwani@nitsri.net
1Corresponding author.
Contributed by the Tribology Division of ASME for publication in the JOURNAL OF TRIBOLOGY. Manuscript received January 21, 2017; final manuscript received May 6, 2017; published online July 21, 2017. Assoc. Editor: Dae-Eun Kim.
J. Tribol. Jan 2018, 140(1): 011604 (21 pages)
Published Online: July 21, 2017
Article history
Received:
January 21, 2017
Revised:
May 6, 2017
Citation
Khabale, D., and Wani, M. F. (July 21, 2017). "Tribological Characterization of AZ91 and AE42 Magnesium Alloys in Fretting Contact." ASME. J. Tribol. January 2018; 140(1): 011604. https://doi.org/10.1115/1.4036922
Download citation file:
Get Email Alerts
Cited By
Related Articles
Closure to “Discussion of ‘Wear Rate and Entropy Generation Sources in a Ti6Al4V–WC/10Co Sliding Pair’” (2017, ASME J. Tribol., 139(6), p. 061608)
J. Tribol (March,2018)
Experimental Investigations on the Tribological Performance of Electric Discharge Alloyed Ti–6Al–4V at 200–600 °C
J. Tribol (June,2020)
Effect of Laser Shock Peening on the Wear–Corrosion Synergistic Behavior of an AZ31B Magnesium Alloy
J. Tribol (April,2020)
Fully Coupled Frictional Contact Using Elastic Halfspace Theory
J. Tribol (July,2008)
Related Proceedings Papers
Related Chapters
Surface Analysis and Tools
Tribology of Mechanical Systems: A Guide to Present and Future Technologies
On the Evaluation of Thermal and Mechanical Factors in Low-Speed Sliding
Tribology of Mechanical Systems: A Guide to Present and Future Technologies
Effectiveness of Minimum Quantity Lubrication (MQL) for Different Work Materials When Turning by Uncoated Carbide (SNMM and SNMG) Inserts
Proceedings of the 2010 International Conference on Mechanical, Industrial, and Manufacturing Technologies (MIMT 2010)