Abstract
Initiation fracture toughness of some selected steels used for transmission line hardware components was measured using an AC potential drop method. The moderate upsetting due to the forging operation of the 1541 bar material increased the initiation fracture toughness by up to 27%, as compared to that of the rolled bar. Initiation fracture toughness of the oil-quenched 4140 steel increased by 60% with the decrease in hardness from Rc 40 to 28.
Issue Section:
Technical Notes
References
1.
Blanchette
, Y.
and Nguyen-Duy
, P.
, “Application of Fracture Mechanics in the Design of Transmission Line Hardware Components
,” Canadian Electrical Association
, Montreal, CEA Report 285 T 585, 08
1991
.2.
Bhuyan
, G.
and Carter
, D.
, “Fracture Properties of Ferrous Alloys Utilized for Transmission Line Hardware Components
,” Canadian Electrical Association
, Montreal, CEA Report 299 T 782, 09
1994
.3.
CAN/CSA G40.21-M92, “
Structural Quality Steels
,” National Standards of Canada
, 1992
.4.
Okumura
, N.
, Venkatasubramanian
, T. V.
, Vnvala
, B. A.
, and Baker
, T. J.
, “Application of the AC Potential Drop Technique to the Determination of Tough Ferritic Steels
,” Engineering Fracture Mechanics
0013-7944, Vol. 14
, 1981
, p. 7.
This content is only available via PDF.
All rights reserved. This material may not be reproduced or copied, in whole or in part, in any printed, mechanical, electronic, film, or other distribution and storage media, without the written consent of ASTM International.
You do not currently have access to this content.