Sachs’ method is an experimental procedure used primarily in the determination of residual stresses in autofrettaged thick cylinders. In its usual form it involves fixing axial and hoop direction strain gauges to the OD of a tube; strain readings are then obtained after each incremental removal of material from the bore. Sachs’ analysis assumes that the remaining tube unloads in linear-elastic fashion throughout the process and that superposition may therefore be employed to quantify the residual stresses within the original tube. By numerical simulation of two complete Sachs’ experimental sequences with “open end” conditions it is demonstrated that the assumption of elastic unloading is invalidated by the Bauschinger effect. Sachs’ method thereby overestimates compressive residual bore hoop stresses in a typical tube by between 24% and 43%. If used as the basis for cyclic pressurization fatigue lifetime predictions with pre-existing cracks, such discrepancies will cause overestimates in fatigue lifetime of an order of magnitude. Sachs’ experimental procedure is therefore not recommended as a reliable or conservative method for determination of residual stress.
Skip Nav Destination
e-mail: tony_parker@tesco.net
Article navigation
Technical Papers
A Critical Examination of Sachs’ Material-Removal Method for Determination of Residual Stress
Anthony P. Parker
e-mail: tony_parker@tesco.net
Anthony P. Parker
Royal Military College of Science, Cranfield University, Swindon, SN6 8LA, England
Search for other works by this author on:
Anthony P. Parker
Royal Military College of Science, Cranfield University, Swindon, SN6 8LA, England
e-mail: tony_parker@tesco.net
Contributed by the Pressure Vessels and Piping Division for publication in the JOURNAL OF PRESSURE VESSEL TECHNOLOGY. Manuscript received by the PVP Division November 12, 2003; revision received December 12, 2003. Associate Editor: G. C. Slagis.
J. Pressure Vessel Technol. May 2004, 126(2): 234-236 (3 pages)
Published Online: May 5, 2004
Article history
Received:
November 12, 2003
Revised:
December 12, 2003
Online:
May 5, 2004
Citation
Parker, A. P. (May 5, 2004). "A Critical Examination of Sachs’ Material-Removal Method for Determination of Residual Stress ." ASME. J. Pressure Vessel Technol. May 2004; 126(2): 234–236. https://doi.org/10.1115/1.1689357
Download citation file:
Get Email Alerts
Related Articles
Stress Intensity Factors for a Curved-Front Internal Crack in an Autofrettaged Tube With Bauschinger Effect
J. Pressure Vessel Technol (May,2004)
A Re-Autofrettage Procedure for Mitigation of Bauschinger Effect in Thick Cylinders
J. Pressure Vessel Technol (November,2004)
Stress Intensity Factors for Internal Straight and Curved-Fronted Cracks in Thick Cylinders
J. Pressure Vessel Technol (May,2006)
3-D Stress Intensity Factors for Internal Cracks in an Overstrained Cylindrical Pressure Vessel—Part II: The Combined Effect of Pressure and Autofrettage
J. Pressure Vessel Technol (February,2001)
Related Proceedings Papers
Related Chapters
New Guidelines on Assessing the Risk of Fatigue Failure and Remaining Life of Ageing Pressure Vessels:
Ageing and Life Extension of Offshore Facilities
Influence of Bauschinger Effect on Residual Stress and Fatigue Lifetimes in Autofrettaged Thick-Walled Cylinders
Fatigue and Fracture Mechanics: 29th Volume
Start-Up, Shutdown, and Lay-Up
Consensus on Pre-Commissioning Stages for Cogeneration and Combined Cycle Power Plants