This paper deals with some general properties of a ductile fracture criterion, which generalizes two ductile fracture criteria conventionally adopted for metal forming analysis and design. The results are valid for a wide class of material models applicable to both cold and hot metal formings. It is expected that the theoretical features of the fracture criterion emphasized in the present paper can be useful for its experimental verification or for determining its parameters from the experiment.
Issue Section:
Technical Briefs
1.
Atkins
, A. G.
, 1996, “Fracture in Forming
,” J. Mater. Process. Technol.
0924-0136, 56
(1–4
), pp. 609
–618
.2.
Shabara
, M. A.
, El-Domiaty
, A. A.
, and Kandil
, M. A.
, 1996, “Validity Assessment of Ductile Fracture Criteria in Cold Forming
,” J. Mater. Eng. Perform.
1059-9495, 5
(4
), pp. 478
–488
.3.
Hambli
, R.
, and Reszka
, M.
, 2002, “Fracture Criteria Identification Using an Inverse Technique Method and Blanking Experiment
,” Int. J. Mech. Sci.
0020-7403, 44
, pp. 1349
–1361
.4.
Kuhn
, H. A.
, Lee
, P. W.
, and Enturk
, T.
, 1973, “A Fracture Criterion for Cold Forming
,” ASME J. Eng. Mater. Technol.
0094-4289, 95
, pp. 213
–218
.5.
Oh
, S. I.
, and Kobayashi
, S.
, 1976, “Workability of Aluminum Alloy 7075-T6 in Upsetting and Rolling
,” ASME J. Eng. Ind.
0022-0817, 98
, pp. 800
–806
.6.
Gänser
, H. -P.
, Atkins
, A. G.
, Kolednik
, O.
, Fisher
, F. D.
, and Richard
, O.
, 2001, “Upsetting of Cylinders: A Comparison of Two Different Damage Indicators
,” ASME J. Eng. Mater. Technol.
0094-4289, 123
, pp. 94
–99
.7.
Sljapic
, V.
, Hartley
, P.
, and Pillinger
, I.
, 2002, “Observations on Fracture in Axi-Symmetric and Three-Dimensional Cold Upsetting of Brass
,” J. Mater. Process. Technol.
0924-0136, 125–126
, pp. 267
–274
.8.
Vilotić
, D.
, Plančak
, M.
, Čupković
, D.
, Alexandrov
, S.
, and Alexandrova
, N.
, 2006, “Free Surface Fracture in Three Upsetting Tests
,” Exp. Mech.
0014-4851, 46
, pp. 115
–120
.9.
Vilotić
, D.
, Plančk
, M.
, Grbić
, S.
, Alexandrov
, S.
, and Chikanova
, N.
, 2003, “An Approach to Determining the Workability Diagram Based on Upsetting Tests
,” Fatigue Fract. Eng. Mater. Struct.
8756-758X, 26
, pp. 305
–310
.10.
Alexandrov
, S.
, Wang
, P. T.
, and Roadman
, R. E.
, 2005, “A Fracture Criterion of Aluminum Alloys in Hot Metal Forming
,” J. Mater. Process. Technol.
0924-0136, 160
, pp. 257
–265
.11.
Alexandrov
, S.
, and Vilotić
, D.
, 2008, “A Theoretical Experimental Method for the Identification of the Modified Cockroft–Latham Ductile Fracture Criterion
,” Proc. Inst. Mech. Eng., Part C: J. Mech. Eng. Sci.
0954-4062, 222
, pp. 1869
–1872
.12.
Shah
, J. J.
, and Kuhn
, H. A.
, 1986, “An Empirical Formula for Workability Limits in Cold Upsetting and Bolt Heading
,” J. Appl. Metalwork.
, 4
, pp. 255
–261
.13.
Kivivuori
, S.
, 1987, “Assessing Cold Forgeability by the Upsetting Test
,” Scand. J. Metall.
0371-0459, 16
, pp. 98
–102
.14.
Oh
, S. I.
, Chen
, C. C.
, and Kobayashi
, S.
, 1979, “Ductile Fracture in Axisymmetric Extrusion and Drawing. Part 2: Workability in Extrusion and Drawing
,” ASME J. Eng. Ind.
0022-0817, 101
, pp. 36
–44
.15.
Murty
, S. V. S. N.
, Rao
, B. N.
, and Kashyap
, B. P.
, 2004, “Improved Ductile Fracture Criterion for Cold Forming of Spheroidised Steel
,” J. Mater. Process. Technol.
0924-0136, 147
, pp. 94
–101
.16.
Bao
, Y.
, and Wierzbicki
, T.
, 2004, “A Comparative Study on Various Ductile Crack Formation Criteria
,” ASME J. Eng. Mater. Technol.
0094-4289, 126
, pp. 314
–324
.17.
Gouveia
, B. P. P. A.
, Rodrigues
, J. M. C.
, and Martins
, P. A. F.
, 1996, “Fracture Prediction in Bulk Metal Forming
,” Int. J. Mech. Sci.
0020-7403, 38
, pp. 361
–372
.18.
Dodd
, B.
, and Boddington
, P.
, 1980, “The Causes of Edge Cracking in Cold Rolling
,” J. Mech. Work. Technol.
0378-3804, 3
, pp. 239
–252
.19.
Samy
, S. N.
, Saleh
, C. A. R.
, and Ragab
, A. R.
, 2006, “Plastic Flow in Extrusion and Drawing Through Conical and Wedge-Shaped Dies: Prediction of Central Bursting
,” Proc. Inst. Mech. Eng., Part C: J. Mech. Eng. Sci.
0954-4062, 220
, pp. 1201
–1210
.20.
Rajak
, S. A.
, and Reddy
, N. V.
, 2005, “Prediction of Internal Defects in Plane Strain Rolling
,” J. Mater. Process. Technol.
0924-0136, 159
, pp. 409
–417
.21.
Sowerby
, R.
, O’Reilly
, I.
, Chandrasekaran
, N.
, and Dung
, N. L.
, 1984, “Materials Testing for Cold Forging
,” ASME J. Eng. Mater. Technol.
0094-4289, 106
, pp. 101
–106
.22.
Sowerby
, R.
, and Chandrasekaran
, N.
, 1984, “The Cold Upsetting and Free Surface Ductility of Some Commercial Steels
,” J. Appl. Metalwork
, 3
, pp. 257
–263
.23.
Ogawa
, N.
, Shiomi
, M.
, and Osakada
, K.
, 2002, “Forming Limit of Magnesium Alloy at Elevated Temperatures for Forging
,” Int. J. Mach. Tools Manuf.
0890-6955, 42
, pp. 607
–614
.Copyright © 2010
by American Society of Mechanical Engineers
You do not currently have access to this content.