An Electroless Ni plating process for aluminum was evaluated and optimized, leading to smooth and uniform nickel growth approaching 28.2 μm/hr. The effects of temperature, and process time were investigated. Nickel bumping die for solder adhesion was performed and the quality of the adhesion between the nickel and aluminum layers was evaluated.