The long-term performance of ferritic/martensitic steel T91 and austenitic 316L in oxygen-containing flowing lead-bismuth eutectic at 550°C was investigated by exposing the materials for up to 15000 h in the CORRIDA loop. The velocity of the liquid-metal flow was 2 m/s and the concentration of dissolved oxygen averaged 1.6×10−6 mass%. The resulting corrosion processes and products were analyzed and quantified using metallographic methods.